Deprecated: $wgMWOAuthSharedUserIDs=false is deprecated, set $wgMWOAuthSharedUserIDs=true, $wgMWOAuthSharedUserSource='local' instead [Called from MediaWiki\HookContainer\HookContainer::run in /var/www/html/w/includes/HookContainer/HookContainer.php at line 135] in /var/www/html/w/includes/Debug/MWDebug.php on line 372
In-situ observation of fatigue crack growth for \({\langle001\rangle}\)-oriented rhombohedral Pb(Mg\(_{1/3}\) Nb\(_{2/3}\))O\(_{3}\)-PbTiO\(_{3}\) ferroelectric single crystal - MaRDI portal

In-situ observation of fatigue crack growth for \({\langle001\rangle}\)-oriented rhombohedral Pb(Mg\(_{1/3}\) Nb\(_{2/3}\))O\(_{3}\)-PbTiO\(_{3}\) ferroelectric single crystal (Q1028744)

From MaRDI portal





scientific article; zbMATH DE number 5576080
Language Label Description Also known as
English
In-situ observation of fatigue crack growth for \({\langle001\rangle}\)-oriented rhombohedral Pb(Mg\(_{1/3}\) Nb\(_{2/3}\))O\(_{3}\)-PbTiO\(_{3}\) ferroelectric single crystal
scientific article; zbMATH DE number 5576080

    Statements

    In-situ observation of fatigue crack growth for \({\langle001\rangle}\)-oriented rhombohedral Pb(Mg\(_{1/3}\) Nb\(_{2/3}\))O\(_{3}\)-PbTiO\(_{3}\) ferroelectric single crystal (English)
    0 references
    0 references
    6 July 2009
    0 references
    fatigue crack growth
    0 references
    PMN-PT single crystals
    0 references
    reliability
    0 references
    ferroelectrics
    0 references

    Identifiers