Deprecated: $wgMWOAuthSharedUserIDs=false is deprecated, set $wgMWOAuthSharedUserIDs=true, $wgMWOAuthSharedUserSource='local' instead [Called from MediaWiki\HookContainer\HookContainer::run in /var/www/html/w/includes/HookContainer/HookContainer.php at line 135] in /var/www/html/w/includes/Debug/MWDebug.php on line 372
On the calculation of stress intensity factors for surface cracks in welded pipe--plate and tubular joints - MaRDI portal

On the calculation of stress intensity factors for surface cracks in welded pipe--plate and tubular joints (Q1399227)

From MaRDI portal





scientific article; zbMATH DE number 1956787
Language Label Description Also known as
English
On the calculation of stress intensity factors for surface cracks in welded pipe--plate and tubular joints
scientific article; zbMATH DE number 1956787

    Statements

    On the calculation of stress intensity factors for surface cracks in welded pipe--plate and tubular joints (English)
    0 references
    0 references
    0 references
    30 July 2003
    0 references
    Stress intensity factor
    0 references
    weight function
    0 references
    surface crack
    0 references
    pipe-plate joint
    0 references
    tubular joint
    0 references
    finite element method
    0 references

    Identifiers